BLACKENING COATING

Put the metal parts into the solution of NaOH, NaNO2 and other potions. At a
certain temperature, the parts will react chemically to produce a thin blue
(black) oxide film. Blackening can be divided into normal temperature
blackening and high temperature blackening. Generally, the surface oxide film
of normal temperature blackening is relatively thin, and the effect of
secondary blackening is better. The blackening treatment temperature at high
temperature is about 135 ° to 155 ° and the blackening effect is also the
best.

What Is Blackening For Metal?
Metal blackening is a common CNC surface finish treatment process. The purpose
of blackening is to prevent rust on the metal surface. There are two kinds of
metal blackening: alkaline heating blackening and normal temperature
blackening. The problem of checking the antirust effect may occur due to
process problems in normal temperature blackening.

How Do You Blacken Metal?
The process flow of metal blackening is as follows:

Degreasing: Boil the parts in degreasing solution for 20~30 minutes at 80~100
℃.

Cold water cleaning: rinse with flowing clean water.

Pickling: wash with hydrochloric acid solution at room temperature for no more
than 30 seconds.

Blackening (put the blackening liquid in a stainless-steel container and heat
the bottom with an electric furnace)

Water washing: wash with flowing cold water or warm water for 30-60 seconds.

Boiling water cleaning: 2-5 minutes.

Saponification treatment: temperature 80~90°, time 2-3 minutes.

Immerse in oil: immerse in transformer oil or spindle oil at about 80° for 1-3
minutes, and then the finished product is cleaned.

Minimum Order: 1 pieces

BLACKENING COATING
Enlarge Click to Enlarge
SOURCE: Import-Export Bulletin Board (https://www.imexbb.com/)
Report Abuse

Post an Offer to Sell

© 1996-2010 IMEXBB.com. All rights reserved.

IMEXBB.com